热风炉用低蠕变高铝砖
项目 \ 指标 \ 牌号 | 高铝砖 | 低蠕变高铝砖 | |||
RL-65 | RL-55 | RL-48 | RDLZ-75 | RDLZ-65 | |
AL2O3 % | ≥65 | ≥55 | ≥48 | ≥75 | ≥65 |
体积密度g/cm3 BD | ≥2.75 | ≥2.70 | |||
显气孔率% AP | ≤24 | ≤24 | ≤24 | ≤18 | ≤19 |
常温耐压强度MPa CCS | ≥50 | ≥44.5 | ≥39.8 | ≥80 | ≥80 |
耐火度℃ | ≥1790 | ≥1790 | ≥1750 | >1790 | >1790 |
荷重软化温度℃RUL | ≥1500 | ≥1470 | ≥1420 | ≥1620 | ≥1590 |
重烧线变化1500℃×2h% | +0.0 -0.4 | +0.0 -0.4 | (1450℃×2h)+0.0-0.4 | 0.2 | 0.4 |
蠕变率% | (1450℃×50h)-0.50 | (1450℃×50h)-0.80 |